Indalloy® 224 In-Sn-Zn Solder Alloy
Subcategory: Indium Alloy; Tin Alloy; Nonferrous Metal
Key Words: lead free, eutectic solder
Material Notes: Pb free solder, high dross due to Zn. Information provided by the manufacturer, Indium Corporation.
| Available Properties |
- Density
- Melting Point
- Solidus
- Liquidus
|
|
|
|