Indalloy® 121 Sn-Ag Solder Alloy
Subcategory: Tin Alloy; Nonferrous Metal; Solder/Braze Alloy
Material Notes: Binary solder has history of use, marginal wetting. Standard tin-silver eutectic solder with wide application when lead-based solders do not meet temperature, strength or safety requirements. Not recommended against gold-plated surfaces. Excellent for step soldering with #42, #106, #165 and #171. Information provided by the manufacturer, Indium Corporation.