Indalloy® 209 Sn-Ag-Sb Solder Alloy
Subcategory: Silver Alloy; Tin Alloy; Nonferrous Metal; Solder/Braze Alloy
Material Notes: Low temperature die attach alloy. Has very high tensile strength. Old Motorola die attach solder; very brittle. Information provided by the manufacturer, Indium Corporation.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- CTE, linear 20°C
- Melting Point
- Solidus
- Liquidus
|
|
|
|