Indalloy® 150 Pb-In Solder Alloy
Subcategory: Indium Alloy; Lead Alloy; Nonferrous Metal; Solder/Braze Alloy
Material Notes: Indalloys #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics of lead-indium as well as good thermal fatigue properties. Information provided by the manufacturer, Indium Corporation.