Indalloy® 164 Pb-In-Ag Solder Alloy
Subcategory: Lead Alloy; Nonferrous Metal; Solder/Braze Alloy
Material Notes: This alloy is very useful in the 300°C range. It has particularly good thermal fatigue properties as well as the minimal gold leaching properties of indium-lead alloys. Often used in reducing atmospheres. Information provided by the manufacturer, Indium Corporation.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Shear Strength
- Electrical Resistivity
- CTE, linear 20°C
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |