Indalloy® 249 91.8Sn/3.4Ag/4.8Bi Lead-Free Solder Alloy
Subcategory: Tin Alloy; Nonferrous Metal; Solder/Braze Alloy
Material Notes: Board & component metallizations must be Pb-free. U.S. Patent 5,439,639 (ICA Licensed Sandia Patent) Information provided by the manufacturer, Indium Corporation.
| Available Properties |
- Melting Point
- Solidus
- Liquidus
|
|
|
|