GlidCop® AL-60 Dispersion Strengthened Copper
Subcategory: Metal Matrix Composite; Copper Alloy; Nonferrous Metal
Key Words: OMG Americas; MMC; Metal Matrix Composite
Material Notes: GlidCop® AL-60 is copper that is dispersion strengthened with 1.1 wt% ultrafine particles of aluminum oxide. It is produced using an internal oxidation powder metallurgy process whereby aluminum oxide is formed in the Cu matrix. The matrix is hardened while the Cu electrical and thermal conductivity are minimally lowered. The aluminum oxide particles are very thermally stable and remain effective in strengthening the copper matrix and resisting grain coarsening even after very long exposures to high temperatures as in brazing or high temp duty cycles. GlidCop® is available with three different levels of Al2O3. Increasing the Al2O3 levels will increase strength but decrease conductivities. All three grades can be further strengthened by cold work. GlidCop® is available in a wide range of extruded and drawn shapes and sizes, including rounds, rectangles, wire, plates, tubes, and strip. Available on a limited basis in powder form. Information provided by OMG Americas.
| Available Properties |
- Tensile Strength, Yield
- Electrical Resistivity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|