Osprey Metals 304L/MA Master Alloy Stainless Steel Powder (Grade 95% - 16)
Subcategory: Stainless Steel; T 300 Series Stainless Steel; Metal
Key Words: Powder metallurgy, MasterAlloy, Metal Powder, Metal Injection Molding, MIM, Microfine
Material Notes: Particle size distribution 1-250 microns. Typical distribution:- 98% < 22 microns
- 95% < 16 microns
- 80% < 10 microns
- 26% < 5 microns
Mean size is 6.7 microns. Master alloy blended with 2 parts iron to produce 304L alloy after sintering. SHAPE: Predominantly spherical PACKAGING: 4 & 20 Kg. Chemical composition and particle size distribution can be adjusted to suit customers' requirements. The specifications listed are subject to the benefits and scrutiny of Osprey's accreditation to ISO 9001. If the product delivered does not substantially meet the specification, Osprey will replace it. Osprey's liability is limited to the cost of replacement. Information provided to MatWeb by Osprey Metals.
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|