Osprey Metals Co 400 Cobalt Thermal Spray Powder
Subcategory: Nonferrous Metal; Cobalt Alloy
Key Words: PowderMetallurgy, Thermal Spray, Non Self Fluxing, Metal Powder, Plasma Spray, HVOF
Material Notes: Particle size distribution 1-250 microns. High quality gas atomized powders for plasma and high velocity thermal spray systems using a well established range of cobalt based alloys, formulated to produce high integrity coatings. The alloys are selected to give a wide range of wear resistant properties for abrasion, corrosion and erosion at elevated temperatures. Information provided to MatWeb by Osprey Metals.
|
|
|