Outokumpu 4016 Ferritic Stainless Steel
Subcategory: Stainless Steel; Alloy Steel; Metal; Ferritic
Key Words: EN 1.4016; ASTM 430; JIS SUS 430
Material Notes: Fairly good corrosion resistant formable steel in mildly corrosive environments. Oxidation resistant at elevated temperatures (up to ~800°C). Ductile, does not work harden readily, and is well suited for deep drawing and bending.Applications: Used in a variety of interior applications where material cost and corrosion performance are important factors. Typical applications include: - Washing machines
- Dish-washers
- Sinks
- Electrical tie-wire
- Vine wire
- Sink rims
- Counter tops
- Cooker hoods
- Refrigerators
- Tableware
- Restaurant equipment
- Indoor cladding
- Flue-gas ducts
Available in cold rolled narrow strip, bar, and rod forms.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Yield
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|