Outokumpu 2205 Duplex Stainless Steel
Subcategory: Stainless Steel; Alloy Steel; Metal
Key Words: EN 1.4462; ASTM S32205, S31803; JIS SUS 329J3L
Material Notes: Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: - Pulp and paper industry
- Desalination plants
- Flue-gas cleaning
- Cargo tanks and pipe systems in chemical tankers
- Seawater systems
- Firewalls and blast walls on offshore platforms
- Bridges
- Components for structural design
- Storage tanks
- Pressure vessels
- Heat exchangers
- Water heaters
- Rotors, impellers and shafts
Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Yield
- Modulus of Elasticity
- Poissons Ratio
- Fatigue Strength
- Impact Test
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Annealing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|