Outokumpu 4567 Austenitic Stainless Steel
Subcategory: Stainless Steel; Alloy Steel; Metal
Key Words: EN 1.4567; ASTM S30430; JIS SUS XM7
Material Notes: Good corrosion resistance with excellent low cold work hardening properties.Applications: Suitable for manufacture of cold headed fasteners. Bar and rod forms.
| Available Properties |
- Density
- Modulus of Elasticity
- CTE, linear 20°C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|