Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel
Subcategory: Stainless Steel; Alloy Steel; Metal
Key Words: EN 1.4571; ASTM 316Ti; JIS SUS 316Ti
Material Notes: Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Yield
- Modulus of Elasticity
- Poissons Ratio
- Impact Test
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|