Outokumpu 4845 High Temperature Austenitic Stainless Steel
Subcategory: Stainless Steel; Alloy Steel; Metal
Key Words: EN 1.4845; ASTM 310S; JIS SUS 310S
Material Notes: Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use over 550°C for equipment and components within: - Iron, steel, and non-ferrous industries
- Engineering industry
- Energy conservation plants
- Cement industry
Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Yield
- Creep Strength
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
- Annealing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|