Outokumpu 4841 High Temperature Austenitic Stainless Steel
Subcategory: Stainless Steel; Alloy Steel; Metal
Key Words: EN 1.4841; ASTM 314
Material Notes: Variant of 1.4845 with an increased silicon content which enhances the steel`s resistance to oxidation/corrosion but has also made it more susceptible to embrittlement.Applications: Heat and creep resistance. For use over 550°C for equipment and components within: - Iron, steel, and non-ferrous industries
- Engineering industry
- Energy conservation plants
- Cement industry
Available in hot rolled plate (Quarto) form.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Yield
- Creep Strength
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
- Annealing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|