Alloy 718, 15% Cold Worked
Subcategory: Superalloy; Nickel Base
Key Words: NACE MR-01-75, ASTM B626; AFNOR NC 19 Fe Nb, UNS N07718, AMS 5596, AMS 5597, AMS 5662, AMS 5664, AMS 5832, AMS 5589, AMS 5590, Werkstoff Nr. 2.4668; WL Nr. 2.4668; MIL-N-24469; NACE MR-01-75; AECMA Pr EN 2404, 2405, 2407, 2408, 2952, 2961, 3219
Material Notes: 15% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy. Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes International.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Electrical Resistivity
- Magnetic Permeability
- Curie Temperature
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|