Alloy X, 15% Cold Worked
Subcategory: Superalloy; Nickel Base
Key Words: UNS N06002, AMS 5536, AMS 5588, AMS 5754, AMS 5798, AMS 5799, AMS 5888
Material Notes: 15% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy. Data provided by High Performance Alloys, Inc., Allvac, and Haynes International.