Reade Advanced Materials Wood's Metal Alloy (Sn + Pb + Bi + Cd)
Subcategory: Bismuth Alloy
Key Words: Cerro bend, Wood's Metal
Material Notes: Description: A low melting fusible alloy. Physical Properties Available: Various granulations are available. Used in heating baths in laboratories, antifriction metals, and solders. Information provided by Reade Advanced Materials.
| Available Properties |
- Heat of Fusion
- Specific Heat Capacity
- Melting Point
|
|
|
|
| Property Data |