RSP Technology Aluminum RSA-905
Subcategory: Aluminum Alloy; Nonferrous Metal
Close Analogs: Aluminum composition calculated by balance.
Key Words: Aluminium
Material Notes: Information provided by RSP Technology BV RSA-905 is a robust alloy. No heat treatment is needed to realize properties. Uses at room temperature include constructions, bicycle parts, and skate frames. Uses at temperature up to 200°C include compressor wheels, conrods and fasteners. High temperature applications include pistons.
| Available Properties |
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- CTE, linear 20°C
|
|
|
|