Stellite® alloy 21

 

Subcategory: Superalloy; Cobalt Base

Close Analogs: Vitallium, ASTM F75, HS21

Key Words: AMS 5385, ASTM A732 Gr.21, MIL-C-13358, Deloro Stellite Inc.

Material Notes:
Cobalt content as balance. Excellent high temperature strength, high toughness. Solution treat at 1191-1204°C, rapid air cool, age between 538-871°C to increase hardness and strength at the expense of impact and ductility.

Applications: turbine blades and vanes, hot die applications, components in combustion or exhaust systems where high strength to 816°C and oxidation to 1093°C is required, used as medical and dental components as well as remelt stock.

X

Corrosion:Excellent resistance to body fluids and has been used for medical implants, dental fixtures, and surgical equipment. Good resistance to cavitation corrosion.

Machinability: best in solution treated condition. Carbide tipped tools and low speeds and feeds should be used to avoid work hardening. Lubrication is normally used.

X

Wear: Excellent galling resistance when self-mated or mated with Stellite alloy-6. Resistance to cavitation erosion nearly as good as Stellite alloy 6 and as good or better at high loads. Lower carbon content makes it inferior to Stellite alloy 6 for low stress abrasion resistance.

Data provided by the manufacturer, Deloro Stellite Inc.

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Knoop
  • Hardness, Rockwell A
  • Hardness, Rockwell B
  • Hardness, Rockwell C
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Compressive Yield Strength
  • Charpy Impact
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。