Stellite® alloy 31 PM, cast, tested at 538°C (1000°F)
Subcategory: Superalloy; Cobalt Base
Key Words: Deloro Stellite Inc.
Material Notes: Cobalt content as balance, typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous wear parts. Data provided by the manufacturer, Deloro Stellite Inc.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- CTE, linear 250°C
- CTE, linear 500°C
|
|
|
|