Tribaloy® alloy 745
Subcategory: Superalloy; Nickel Base
Key Words: Deloro Stellite Inc.
Material Notes: Nickel content as balance. Age-hardened, highly alloyed, nickel base alloy in the casting form. Hardened by the presence of intermetallic compounds in the highly alloyed matrix. Unique combination of corrosion and wear resistant.Applications: Used in high temperature, highly corrosive environments where good wear resistance in needed. Data provided by the manufacturer, Deloro Stellite Inc.
| Available Properties |
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell A
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Elongation at Break
- Compressive Yield Strength
|
|
|
|