Sandvik H6F Cemented Carbide for Can Tooling
Subcategory: Metal Matrix Composite; Carbide; Tungsten Alloy; Nonferrous Metal
Material Notes: SANDVIK Grade H6F:6% Co, 93.7% tungsten carbide (WC) and 0.3% other.Extrafine carbide grain size.High wear resistance.Medium corrosion resistance.Information provided by Sandvik
| Available Properties |
- Density
- Hardness, Rockwell A
- Hardness, Vickers
- Compressive Strength
- Fracture Toughness
- Corrosion Resistance, 1-10
- Wear Resistance, 0-10
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|