Sandvik H6N 6% Cobalt Binder Cemented Carbide, Seal Grade
Subcategory: Metal Matrix Composite; Carbide; Tungsten Alloy; Nonferrous Metal
Material Notes: Sandvik seal grade H6N is a standard/straight cobalt binder grade. This grade shows excellent wear resistance combined with high toughness.
Due to the cobalt binder, this grade is not recommended for applications in corrosive environments.Features: 6% cobalt binder, 94% tungsten carbide. The carbide grain size is medium.Very good wear resistanceHigh toughnessRelatively low to medium corrosion resistance –particularly to aqueous solutions, due to the cobalt binder.Good brazabilityInformation provided by Sandvik
| Available Properties |
- Density
- Hardness, Rockwell A
- Hardness, Vickers
- Rupture Strength
- Compressive Strength
- Corrosion Resistance, 1-10
- Wear Resistance, 0-10
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|