Sandvik H11N 11% Cobalt Binder Cemented Carbide, Seal Grade
Subcategory: Metal Matrix Composite; Carbide; Tungsten Alloy; Nonferrous Metal
Material Notes: Sandvik seal grade H11N has very high toughness. Due to the cobalt binder, this grade is not recommended for applications in corrosive environments.Features: 11% cobalt and 89% tungsten carbide. The grain size is medium.Very high toughnessRelatively low wear resistanceRelatively low corrosion resistance –due to the cobalt binder.Good brazabilityInformation provided by Sandvik
| Available Properties |
- Density
- Hardness, Rockwell A
- Hardness, Vickers
- Rupture Strength
- Compressive Strength
- Corrosion Resistance, 1-10
- Wear Resistance, 0-10
|
|
|
|