Sandvik C10C Coarse Grained Cemented Carbide, Seal Grade
Subcategory: Metal Matrix Composite; Carbide; Tungsten Alloy; Nonferrous Metal
Material Notes: Sandvik seal grade C10C has been developed for seal ring applications requiring good corrosion resistance, high thermal conductivity and excellent mechanical properties. Sandvik C10C also features high capacity for dry running of the seal.Features: 10% alloyed binder and 90% tungsten carbide with coarse grain size.High resistance to corrosion due to the alloyed binder.Relatively low wear resistance.High thermal conductivity which means good resistance to thermal cracks.High toughness.Good brazability.Information provided by Sandvik
| Available Properties |
- Density
- Hardness, Rockwell A
- Hardness, Vickers
- Rupture Strength
- Compressive Strength
- Corrosion Resistance, 1-10
- Wear Resistance, 0-10
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|