Sandvik H6F Extra-fine Grain Cemented Carbide for Printed Circuit Board Printing
Subcategory: Metal Matrix Composite; Carbide; Tungsten Alloy; Nonferrous Metal
Material Notes: SANDVIK H6F extra-fine grain cemented carbide grades has been developed to meet the exacting demands placed on solid carbide tooling by modern technology. SANDVIK extra-fine grain cemented carbide grades are true sub micron grain size tungsten carbide alloys. The tungsten carbide grain size is 0.8 µm, which is precisely controlled. These grades offer an excellent combination of strength and toughness. In addition, a special additive maximizes corrosion resistance without loss of tough ness. SANDVIK grade H6F incorporates 6% cobalt (Co) and 94% tungsten carbide (WC). SANDVIK grade H6F is recommended for solid carbide rotary tool applications in the ISO K05/K10 range with special advantages where exceptionally sharp edge profiles are demanded. Information provided by Sandvik
| Available Properties |
- Density
- Hardness, Rockwell A
- Hardness, Vickers
- Rupture Strength
- Compressive Strength
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|