Sandvik DH40 Cemented Carbide for Woodworking
Subcategory: Metal Matrix Composite; Carbide; Tungsten Alloy; Nonferrous Metal
Material Notes: The DH family of grades offers two innovations based on the latest Sandvik developments: The unique grain size distribution is optimized to improve the toughness and the micro crack resistance The composition of the DH grades includes specific additions to increase the thermal resistance (thermal cycling fatigue), and the corrosion/oxidation resistanceThis combination of innovations gives the DH grades a high edge retention and crack resistance. These properties, combined with a good brazeability and grindibility, allow the DH grades family to be very efficient when looking at cost/performance ratio. Features: Medium grain size Moderate to medium abrasion resistance High impact strength Binderphase content 11%Codes: ISO K40 Information provided by Sandvik
| Available Properties |
- Density
- Hardness, Rockwell A
- Hardness, Vickers
- Fracture Toughness
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|