Sandvik DC03 Cemented Carbide for Woodworking
Subcategory: Metal Matrix Composite; Carbide; Tungsten Alloy; Nonferrous Metal
Material Notes: Sandvik DC03 grade has been developed to give superior tool life in demanding applications. This extra fine grain size grade with low binder phase content offers a superior hardness and corrosion/oxidation resistance. The extra fine microstructure of DC03 gives the opportunity to reach superior cutting edge quality. Features: Extra fine grain sizeSuperior abrasion resistanceSuperior cutting edge qualitySuperior corrosion and oxidation resistanceBinderphase content 3%Codes: ISO K01, US C4 Information provided by Sandvik