Sandvik KANTHAL Kanthal D Resistance Ribbon
Subcategory: Aluminum Alloy; Iron Base; Metal
Material Notes: KANTHAL D is a ferritic FeCrAl alloy which is used at wire temperatures up to 1300°C (2370°F). It is used in domestic appliances as well as in industrial applications.Typical applications for KANTHAL D are in metal sheathed tubular elements for dishwashers, in elements embedded in ceramics forpanel heaters, in cartridge elements in metal dies, in heating cables and rope heaters in defrosting and de-icing elements, in mica elements used in irons, in quartz tube heaters for space heating, industrial infrared dryers, in coils on molded ceramic fibre for boiling plates with ceramic hobs, in bead insulated coils for panel heaters, in suspended coil elements for air heaters in laundry dryers. In industrial applications such as terminals to furnace elements, in porcupine elements for air heating, and in furnace heating elements. Information provided by Sandvik
| Available Properties |
- Density
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Elongation at Break
- Creep Strength
- Modulus of Elasticity
- Poissons Ratio
- Electrical Resistivity
- Curie Temperature
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Emissivity (0-1)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|