Sandvik KANTHAL Nikrothal 60 Resistance Ribbon
Subcategory: Nickel Alloy; Iron Base
Material Notes: NIKROTHAL 60 can be used at operating temperatures up to 1150°C (2100°F). NIKROTHAL 60 has excellent hot strength, good oxidation properties and very good formability. NIKROTHAL 60 has good corrosion resistance except in sulphur containing atmospheres and certain controlled atmospheres. NIKROTHAL 60 is used as electric heating element material in domestic appliances and furnace applications up to high temperatures.Typical applications for NIKROTHAL 60 are in metal sheathed tubular elements used in hot plates, grills, toaster ovens, storage heaters, etc and as suspended coils in air heaters used in clothes dryers, fan heaters, hand dryers. Information provided by Sandvik
| Available Properties |
- Density
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Elongation at Break
- Creep Strength
- Electrical Resistivity
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Emissivity (0-1)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|