Sandvik KANTHAL Alkrothal 720 Resistance Strip
Subcategory: Aluminum Alloy; Iron Base; Metal
Material Notes: ALKROTHAL 720 is a ferritic FeCrAl alloy which is recommended for use at temperatures up to 1000°C (1830°F). Typical applications for ALKROTHAL 720 are in rheostats, braking resistors, etc. It is also used as electrical heating elements in industrial applications. Information provided by Sandvik
| Available Properties |
- Density
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Elongation at Break
- Creep Strength
- Modulus of Elasticity
- Poissons Ratio
- Electrical Resistivity
- Curie Temperature
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Emissivity (0-1)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|