Sandvik KANTHAL Kanthal APMT Seamless tube and pipe
Subcategory: Aluminum Alloy; Iron Base
Material Notes: KANTHAL APMT is an advanced powder metallurgical, dispersion strengthened, ferritic FeCrAlMo alloy which is used at tube temperatures up to 1250°C (2280°F). KANTHAL APMT tubes have good form stability at high temperature. KANTHAL APMT forms an excellent, non-scaling surface oxide, which gives good protection in most furnace environments, i.e. oxidising, sulphurous and carbonaceous gas, as well as against deposits of carbon, ash, etc. The combination of excellent oxidation properties and form stability makes the alloy unique.Typical applications for KANTHAL APMT are as radiant tubes in electrically or gas fired furnaces such as continuous annealing and galvanizing furnaces, seal quench furnaces, holding furnaces and dosing furnaces in the aluminium, zinc, lead industries, thermocouple protection tubes, furnace muffles for sintering applications. Information provided by Sandvik
| Available Properties |
- Density
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Creep Strength
- Rupture Strength
- Modulus of Elasticity
- Poissons Ratio
- Electrical Resistivity
- Curie Temperature
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Emissivity (0-1)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|