Sandvik KANTHAL Kanthal SW 100 Spray Wire
Subcategory: Aluminum Alloy; Iron Base; Metal
Material Notes: KANTHAL SW 100 is a ferritic FeCrAlY alloy wire developed for use in Arc and Flame Spray systems. The trace elements added in this alloy improve the sprayed coatings protective properties. The wire produces dense, well bonding coatings, resistant to high temperature oxidation. Typical applications are as bond coats in high temperature coating systems, protective coatings against sulphur or carbon containing atmospheres, protective coatings against scaling of conventional low alloy steels.Information provided by Sandvik
| Available Properties |
- Density
- Porosity
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- Curie Temperature
- Melting Point
- Deposition efficency, %
- Oxides, %
- Surface Roughness, microns
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|