Sandvik KANTHAL Kanthal SW 210 Spray Wire
Subcategory: Nickel Alloy; Iron Base; Metal
Material Notes: KANTHAL SW 210 is an austenitic NiFeCr alloy developed for use in Arc and Flame Spray systems. The wire produces dense, well bonding coatings resistant to high temperature oxidation. Typical applications are protective coatings against corrosive gases, protection against scaling of conventional low alloy steels, build up coatings for dimensional restoration.Information provided by Sandvik