Sandvik KANTHAL Kanthal SW 806 Spray Wire
Subcategory: Aluminum Alloy; Nickel Alloy; Metal
Material Notes: KANTHAL SW 806 is an austenitic NiAl alloy wire developed for use in Arc and Flame Spray systems. The wire produces dense, well bonding coatings. Typical applications are as bond coats, as protective coatings against high temperature oxidation, protective coatings against scaling of conventional iron base alloys, and as build up coatings for dimensional restoration.Information provided by Sandvik
| Available Properties |
- Density
- Porosity
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Electrical Resistivity
- Melting Point
- Deposition efficency, %
- Oxides, %
- Surface Roughness, microns
|
|
|
|
| Property Data |