Sandvik KANTHAL Kanthal SW 821 Spray Wire
Subcategory: Copper Alloy; Nickel Alloy
Material Notes: KANTHAL SW 821 is a copper-nickel alloy wire developed for use in Arc and Flame Spray systems. The wire produces dense, well bonding coatings. The coatings are resistant against corrosion, typically used in marine and certain chemical applications.Information provided by Sandvik
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Melting Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|