Sandvik KANTHAL Nisil Thermocouple
Subcategory: Nickel Alloy
Material Notes: NISIL is the negative leg of thermocouple type N. This thermocouple is the most recent one among the different types covered by the international standards. It offers higher thermoelectric stability in air above 1000°C and better oxidation resistance than type E, J and K thermocouples. NISIL alloy cannot be exposed to sulphur-containing gases.Information provided by Sandvik
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Electrical Resistivity
- CTE, linear 100°C
- Thermal Conductivity
- Melting Point
- emf, mV, Refrence junction 0°C
|
|
|
|