Sandvik KANTHAL Nicrosil Thermocouple
Subcategory: Nickel Alloy
Material Notes: NICROSIL is the positive leg of thermocouple type N. This thermocouple is the most recent one among the different types covered by the international standards. It offers higher thermoelectric stability in air above 1000°C and a better oxidation resistance in air than type E, J and K thermocouples. NICROSIL alloy cannot be exposed to reducing or alternatively oxidizing and reducing atmospheres or to vacuum.Information provided by Sandvik
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Electrical Resistivity
- CTE, linear 100°C
- Thermal Conductivity
- Melting Point
- emf, mV, Refrence junction 0°C
|
|
|
|