Sandvik KANTHAL Iron Thermocouple
Subcategory: Aluminum Alloy
Material Notes: IRON is the positive leg of thermocouples type J, L, and it is also the positive leg of compensating cables type KCA (WX). Thermocouple type J and L are frequently used because of their high emf output and their low cost. Compensating cables of type KCA are used together with thermocouples of type K.IRON can not be exposed to sulphur containing atmospheres and to temperatures below zero. The alloy is transformed magnetically at 770°C, and a crystallographic transformation occurs at 900°C. Both transformations affect the thermoelectric
properties of the alloy. The wire is supplied copper-coated in order to prevent oxidation. Information provided by Sandvik
| Available Properties |
- Density
- Hardness, Vickers
- Tensile Strength, Ultimate
- Elongation at Break
- Electrical Resistivity
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|