Sandvik KANTHAL Cuprothal WX Thermocouple
Subcategory: Copper Alloy; Nickel Alloy
Material Notes: CUPROTHAL WX is the negative leg of the compensating cable for thermocouples type "K".CUPROTHAL WX must be matched with Iron to meet the reference standards.Information provided by Sandvik