Sandvik KANTHAL Kanthal 60 Thermostatic bimetal
Subcategory: Nickel Alloy; Iron Base
Close Analogs: Composition: - High-expansive component: Designation 440; 6.9% Mn; 17% Ni; 76.1 Fe
- Low-expansive component: Designation Fe; 100% Fe
Material Notes: KANTHAL 60 is a thermostatic bimetal which is recommended for use in the temperature range -20 to +450 °C. Typical applications for KANTHAL 60 are in circuit breakers, motor protection units, thermostats, shower mixers, etc. High-expansive component: 15-7 Alloy (440 Designation, 54.5% of thickness) Low-expansive component: Fe (Fe Designation, 45.5% of thickness) Information provided by Sandvik
| Available Properties |
- Density
- Hardness, Vickers
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Linearity Range, °C
- linearity Temperature Range, °C
- Specific thermal curvature, /K
- Specific deflection, /K
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|