Sandvik KANTHAL Kanthal 145 R 19 Thermostatic bimetal

 

Subcategory: Nickel Alloy; Iron Base

Close Analogs:

Composition:

  • High-expansive component: Designation 440; 6.9% Mn; 17% Ni; 76.1% Fe
  • Low-expansive component: Designation 430; 0.3% Mn; 36.5% Ni; Bal. Fe

Material Notes:
KANTHAL 145 R 19 is a thermostatic bimetal which is recommended for use in the temperature range -20 to +250 °C.In extreme cases it can be used at temperatures up to a maximum of +400 °C.

Typical applications for KANTHAL 145 R 19 are in circuit breakers, motor protection units, ammeters etc.

High-expansive component: 15-7 Alloy(440 Designation, 46% of thickness)

Low-expansive component: Invar 145 Alloy (430 Designation, 46% of thickness)

Intermediate component: Copper (470 Designation, 8% of thickness)

Information provided by Sandvik

Available Properties
  • Density
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Electrical Resistivity
  • CTE, linear 100°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Linearity Range, °C
  • linearity Temperature Range, °C
  • Specific thermal curvature, /K
  • Specific deflection, /K
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。