Sandvik KANTHAL Kanthal 94 S Thermostatic bimetal
Subcategory: Nickel Alloy; Iron Base
Close Analogs: Composition: - High-expansive component: Designation 490; 0.35% Mn; 19% Ni; 7.1% Cr; Bal. Fe
- Low-expansive component: Designation 480; 0.4% Mn; 37.8% Ni; 6.6% Cr; Bal. Fe
Material Notes: KANTHAL 94 S is a stainless steel type thermostatic bimetal which is recommended for use in corrosive environments in the temperature range -20 to +375°C. Typical applications for KANTHAL 94 S are in circuit breakers, motor protection units, thermostats, shower mixers, etc. High-expansive component: 19-7 Alloy(490 Designation, 50% of thickness) Low-expansive component: 38-7 Alloy (480 Designation, 50% of thickness) Information provided by Sandvik
| Available Properties |
- Density
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Linearity Range, °C
- linearity Temperature Range, °C
- Specific thermal curvature, /K
- Specific deflection, /K
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|