Sandvik KANTHAL Kanthal 115 R 09 Thermostatic bimetal
Subcategory: Nickel Alloy; Iron Base
Close Analogs: Composition: - High-expansive component: Designation 440; 6.9% Mn; 17% Ni; 76.1% Fe
- Low-expansive component: Designation 420; 0.95% Mn; 42.9% Ni; Bal. Fe
Material Notes: KANTHAL 115 R 09 is a thermostatic bimetal which is recommended for use in the temperature range -20 to +350 °C.In extreme cases it can be used at temperatures up to a maximum of +400 °C.Typical applications for KANTHAL 115 R 09 are in circuit breakers, motor protection units, thermostats, shower mixers, etc. High-expansive component: 15-7 Alloy(440 Designation, 34.8% of thickness) Low-expansive component: Invar 115 Alloy (420 Designation, 46.1% of thickness) Intermediate component: Copper (470 Designation, 19.1% of thickness) Information provided by Sandvik
| Available Properties |
- Density
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Linearity Range, °C
- linearity Temperature Range, °C
- Specific thermal curvature, /K
- Specific deflection, /K
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|