Sandvik SANMAC 4435 Bar Steel
Subcategory: Nickel Alloy; Alloy Steel; Metal
Material Notes: Sandvik SANMAC 316L, 1.4435, with improved machinability is an austenitic chromium-nickel steel with minimum 2.5% molybdenum.Industrial Categories:Chemical IndustryFood IndustryPetrochemical IndustryPilp and Paper IndustryNuclear IndustryTypical Applications: FlangesValvesFittingsCouplingsRingsSealsBolts and NutsShaftsForgings DiscsInformation provided by Sandvik
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|