Sandvik SANMAC SAF 2205 Bar Steel

 

Subcategory: Stainless Steel; Metal; Austenitic; Ferritic; Duplex

Close Analogs: ASTM A479, A276; EN 1.4462; UNS S31803, S32205

Material Notes:
Sandvik SANMAC SAF 2205™ is a duplex stainless steel (austenitic-ferritic). It is characterised by:

  • high resistance to stress corrosion cracking in chloride-bearing environments
  • high resistance to stress corrosion cracking in environments containing hydrogen sulphide
  • high resistance to general corrosion, pitting and crevice corrosion
  • high mechanical strength – roughly twice the proof strength of austenitic stainless steels excellent machinability
  • good hot-working properties
  • high resistance to erosion corrosion and corrosion fatigue
  • physical properties that offer design advantages
  • good weldability
  • Information provided by Sandvik

    Available Properties
    • Density
    • Hardness, Brinell
    • Tensile Strength, Ultimate
    • Tensile Strength, Yield
    • Tensile Strength, Yield at Elevated Temperature
    • Elongation at Break
    • CTE, linear 100°C
    • Specific Heat Capacity
    • Thermal Conductivity
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。