Sandvik 310-7RE10 Billet
Subcategory: Nickel Alloy; Alloy Steel; Metal
Close Analogs: ASTM 310S, UNS S31008; EN 1.4845
Material Notes: Austenitic stainless steel for high temperatures, AISI type 310SSandvik 7RE10 is an austenitic, stainless chromium-nickel steel of the 25/20 type. It has good resistance to carburisation, sulphidation and oxidation combined with moderate creep strength and structural stability. maximum service temperature in air is 1100°C (2010°F). Information provided by Sandvik
| Available Properties |
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Reduction of Area
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|