Sandvik 316-5R60 Billet
Subcategory: Nickel Alloy; Alloy Steel; Metal
Close Analogs: ASTM 316; UNS S31600; EN 1.4436
Material Notes: Austenitic stainless steel, AISI 316/316HSandvik 5R60 is an austenitic chromium-nickel steel with minimum 2.5% molybdenum and a controlled carbon content in order to obtain improved strength at high temperatures. Information provided by Sandvik
| Available Properties |
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Reduction of Area
|
|
|
|