Sandvik 430-0XC34 Billet
Subcategory: Stainless Steel; Metal; Ferritic
Close Analogs: ASTM 430; UNS S43000; EN 1.4016
Material Notes: Sandvik 430 is an ferritic stainless steel with at least 16% chromium. Due to its ferritic structure 430 has a lower tensile strength, elongation and impact resistance than the austentic stainless steels. The proof strength is somewhat higher.Information provided by Sandvik
| Available Properties |
|
We're sorry, but our sources do not report any other information for this material.
|
|
|
|